Fig. 1

Nanosight results for OFP-filled PCCAs (N = 3 vials). The mean particle size (±SD) was found to be 140 ± 10 nm and the average concentration (±SD) was 1.7 ± 0.1 × 1012 particles/mL
Nanosight results for OFP-filled PCCAs (N = 3 vials). The mean particle size (±SD) was found to be 140 ± 10 nm and the average concentration (±SD) was 1.7 ± 0.1 × 1012 particles/mL